Pseudo-Dynamic Testing, Performance Assessment, and Modeling of Deficient Reinforced Concrete Frames

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pseudo-Dynamic Testing, Performance Assessment, and Modeling of Deficient Reinforced Concrete Frames

Author(s): Haluk Sucuoglu, Wesley Wei-Chih Lin, Barıs¸ Binici, and Pourang Ezzatfar

Publication: Structural Journal

Volume: 111

Issue: 5

Appears on pages(s): 1203-1212

Keywords: deficient frames; lap splices; modeling; performance assessment, pseudo-dynamic testing

DOI: 10.14359/51686922

Date: 9/1/2014

Abstract:
A pair of half-scale, three-story, three-bay concrete bare frames were tested by the pseudo-dynamic (PsD) testing procedure. Both frames represent common deficiencies of non-seismic construction. Continuous column reinforcement in one specimen and insufficient lap splices at the bottom ends of columns in the other specimen were the only significant differences. Measured seismic performances of both frames were assessed by using the rotation and strain-based acceptance criteria of two different seismic codes. Dynamic responses of both frames were also predicted by employing nonlinear frame models. Analytical models of deficient frames were capable of predicting global deformation response, but failed to predict local deformations. Prediction of local deformations in deficient frames can only be improved if joint deformations and hysteretic degradation in member properties are considered directly in the analytical models.