Direct Tensile Behavior of Normal-Strength Concrete at Elevated Temperatures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Direct Tensile Behavior of Normal-Strength Concrete at Elevated Temperatures

Author(s): Eddie Siu-Shu Lam and Shuai Fang

Publication: Materials Journal

Volume: 111

Issue: 6

Appears on pages(s): 641-650

Keywords: direct tensile test; finite element model; high temperature; normal-strength concrete; stress-strain relationship

DOI: 10.14359/51686915

Date: 11/1/2014

Abstract:
The objective of this study is to determine the tensile properties of normal-strength concrete (NSC) at elevated temperatures through direct tensile tests. The specimens were cast in cylindrical cross sections with extended ends according to RILEM TC 129-MHT. After curing, the specimens were heated in a tubular electric furnace at temperatures up to 800°C (1472°F) and then subjected to direct tension under that temperature. At 800°C (1472°F), there is a strength loss of 73% and elastic modulus reduces by 93%. Peak strain increases with increasing temperature up to 700°C (1292°F) and then shows slight reduction between 700 and 800°C (1292 and 1472°F). Complete tensile stress-strain relationships of NSC are proposed and empirical equations for determining direct tensile strength, peak strain, and elastic modulus at different temperatures are provided. Finite element method is applied to simulate the direct tensile tests using the proposed complete stress-strain relationship. Predictions based on the finite element simulations are in good agreement with the test results.