Effect of Elevated Temperature Curing on Compressive Strength and Electrical Resistivity of Concrete with Fly Ash and GGBS

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Elevated Temperature Curing on Compressive Strength and Electrical Resistivity of Concrete with Fly Ash and GGBS

Author(s): Yanbo Liu and Francisco Presuel-Moreno

Publication: Materials Journal

Volume: 111

Issue: 5

Appears on pages(s): 531-542

Keywords: compressive strength; electrical resistivity; elevated temperature curing; SCMs

DOI: 10.14359/51686913

Date: 9/1/2014

Abstract:
This paper presents results regarding the effect of elevated temperature (ET) curing on the compressive strength and electrical resistivity of concrete with slow-reacting supplementary cementitious materials (SCMs). Concrete mixtures with Class F fly ash (FA), ground-granulated blast furnace slag (GGBS), or both were tested. Elevated temperature (ET) curing (in a 36°C [97°F] lime water bath) and room temperature (RT) curing (in a 21°C [70°F] lime water bath) with different durations were investigated. Test results show that the ET curing method can be employed to achieve the specified 28-day compressive strength and resistivity values on concrete with slow-reacting SCMs without compromising the long-term strength and resistivity properties. It is also shown that the use of granite as coarse aggregate as an alternative to limestone can increase concrete’s electrical resistivity but has a modest adverse effect on the compressive strength of not fully hydrated concrete.