Identifying Buildings with High Seismic Risk under Urban Renewal Law in Turkey

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Identifying Buildings with High Seismic Risk under Urban Renewal Law in Turkey

Author(s): Baris Binici, Ahmet Yakut, Sadun Taniser, Guney Ozcebe

Publication: Symposium Paper

Volume: 297

Issue:

Appears on pages(s): 1-16

Keywords: reinforced concrete buildings, seismic assessment, linear elastic procedure.

DOI: 10.14359/51686908

Date: 3/6/2014

Abstract:
A new law known as the "Urban Renewal Law" for risk mitigation was passed in May 2012 with the objective of reducing seismic risk associated with the existing building stock in Turkey. As stated in the law, new provisions are set forth to assess and to identify seismically vulnerable residential buildings as quickly as possible. The buildings that are classified as high risk are either demolished or strengthened. New buildings are constructed through the financing options provided by the government. In this study, first, the technical provisions of seismic risk assessment, based on linear elastic analysis, are briefly described with special emphasis on the deformation limits. Because of the inability of the linear elastic analysis to allow for redistribution, some flexibility is provided on how many vertical load bearing elements are allowed to exceed their performance limits. Afterwards, three case study buildings are analyzed by using the new provisions and ASCE/SEI 41-06 linear elastic procedure. Level and sources of conservatism in the two approaches are critically evaluated.