Quality of Prepackaged Powdered Materials Used in Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Quality of Prepackaged Powdered Materials Used in Construction

Author(s): Peter H. Emmons, Fred R. Goodwin, and Michael M. Sprinkel

Publication: Concrete International

Volume: 36

Issue: 4

Appears on pages(s): 43-47

Keywords: mixture, manufacturing, performance, standard

DOI:

Date: 4/1/2014

Abstract:
Prepackaged, dry, combined materials are commonly used in the United States in construction and repair projects. Users of these materials are experiencing a number of quality issues that are impacting their projects. This article summarizes finding of a workshop organized by the Strategic Development Council (SDC) in September 2013 in Indianapolis, IN, to identify quality and performance issues with these materials and propose solutions to overcome them.