Size Effect in Shear for Steel Fiber-Reinforced Concrete Members without Stirrups

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Size Effect in Shear for Steel Fiber-Reinforced Concrete Members without Stirrups

Author(s): Abdoladel Shoaib, Adam S. Lubell, and Vivek S. Bindiganavile

Publication: Structural Journal

Volume: 111

Issue: 5

Appears on pages(s): 1081-1090

Keywords: crack widths; high-strength concrete; normal-strength concrete; shear; size effect; steel fiber-reinforced concrete (SFRC)

DOI: 10.14359/51686813

Date: 9/1/2014

Abstract:
At the member scale, very few previous tests reported for shear-critical steel fiber-reinforced concrete (SFRC) members have examined specimens with depths greater than 300 mm (11.8 in.), preventing a detailed assessment of the so-called size effect in shear for SFRC. This paper reports on laboratory results of 12 SFRC specimens with an overall height from 308 to 1000 mm (12.1 to 39.4 in.), and a constant shear span-effective depth ratio of 3. Specimens contained normal or high-strength SFRC with 1% volume fraction of hooked-end steel fibers and different longitudinal reinforcement ratios, but no stirrups. The test results show that the steel fibers increase the shear capacity relative to geometrically similar reinforced plain concrete members. The normalized shear stress at failure, however, was observed to decrease as the member depth increased, indicating that a size effect in shear occurs in SFRC members without stirrups. Modifications to the ACI 318-11 provisions for shear in SFRC members are proposed.