Title: Resistivity versus Time Due to Concrete Composition and Exposure to Various Curing Regimes

Author(s): Francisco Presuel-Moreno

Publication: Web Session

Volume: Moreno.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/21/2013

Abstract:
Electrical methods such as surface resistivity, bulk resistivity, and electro-impedance spectroscopy are becoming more prominent to monitor concrete condition in laboratory and field applications, as illustrated through increased interest from infrastructure management agencies and the commercial availability of testing equipment sets. This session will present recent advances of such technology with potential application to nondestructive testing (NDT) and in-place structural monitoring for concrete.