Title: Microsphere-Based Admixture for Durable Concrete

Author(s): Bury, Mark A.; Ong, Frank; Attiogbe, Emmanuel; Nmai, Charles; and Smith, James

Publication: Concrete International

Volume: 36

Issue: 3

Appears on pages(s): 59-63

Keywords: air content, dosage, spacing factor, strength

DOI:

Date: 3/1/2014

Abstract:
BASF has developed a liquid microsphere-based admixture. At a dosage of 1% by volume of concrete, this new admixture will protect concrete exposed to cyclic freezing and thawing under saturated conditions. Full-scale fields trials using ready mixed concrete from both dry-batch and central-batch plants show that microsphere-treated concrete is easy to place and finish.