Abstract:
The principal aim of this paper is to investigate the effect of sand grading, surface morphology, and content on the rheological prop¬erties—that is, yield stress and plastic viscosity—of fresh mortar. Mortars were produced from four different types of sand at two volumetric cement-sand ratios of 1/0.9 and 1/0.6. Each blend was prepared with five water-cement ratios of 0.60, 0.55, 0.50, 0.45, and 0.40. The rheometer was used to determine yield stress and plastic viscosity parameters of each cement paste and mortar. Test results show that the relative yield stress and plastic viscosity of mortar to cement paste is inversely proportional to the excess paste thickness up to low values, below which the surface texture of sand particles becomes significant.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer