Simplified Methods for Crack Risk Analyses of Early Age Concrete Part 2: Restraint Factors for Typical Case Wall-on-Slab

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Simplified Methods for Crack Risk Analyses of Early Age Concrete Part 2: Restraint Factors for Typical Case Wall-on-Slab

Author(s): Majid Al-Gburi, Jan –Erik Jonasson, S. T. Yousif, Martin Nilsson

Publication: NCR

Volume: 46

Issue: 3

Appears on pages(s): 39-56

Keywords: Restraint curves, early age concrete, wall-on-slab, artificial neural network

DOI:

Date: 12/15/2012

Abstract:
Existing restraint curves have been applied to the method of artificial neural networks (ANN) to model restraint in the wall for the typical structure wall-on-slab. It has been proven that ANN is capable of modeling the restraint with good accuracy. The usage of the neural network has been demonstrated to give a clear picture of the relative importance of the input parameters. Further, it is shown that the results from the neural network can be represented by a series of basic weight and response functions. Thus, the results can easily be made available to any engineer without use of complicated software.