Flexural Testing of Reinforced Concrete Beams with Recycled Concrete Aggregates (with Appendix)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Testing of Reinforced Concrete Beams with Recycled Concrete Aggregates (with Appendix)

Author(s): Thomas H.-K. Kang, Woosuk Kim, Yoon-Keun Kwak, and Sung-Gul Hong

Publication: Structural Journal

Volume: 111

Issue: 3

Appears on pages(s): 607-616

Keywords: beams; flexural strength; high-strength concrete; recycled concrete aggregate; recycling

DOI: 10.14359/51686622

Date: 5/1/2014

Abstract:
Owing in part to the fact that appropriate structural design guides for recycled concrete materials have not been established, only approximately 14% of all waste concrete is made into aggregate and recycled. This is an inefficient method of recycling the concrete materials, under-utilizing an important and valuable asset. To promote the use of recycled concrete aggregates (RCAs), flexural tests of 28 reinforced high-strength and normal-strength concrete beams were performed. The main objectives of this research were the structural investigation of flexural performance and the evaluation of the potential application of RCA for concrete structures. In comparing the RCA specimens to the natural aggregate specimens, the overall crack patterns were similar to each other. The flexural behavior was also not affected significantly by the use of RCA up to 30% RCA replacement ratio. The current test data and data from other researchers’ studies were examined in evaluating the flexural strength of reinforced concrete beams with RCA.