Concrete Q & A: Concrete Cover Tolerances

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q & A: Concrete Cover Tolerances

Author(s):

Publication: Concrete International

Volume: 36

Issue: 2

Appears on pages(s): 75-76

Keywords:

DOI:

Date: 2/1/2014

Abstract:
Q. When inspecting bar placements, I’ve been confronted by contractors that argue that bars can be placed as far as 1 to 2 in. (25 to 51 mm) beyond the specified cover. In other words, they say that the tolerance on cover only limits the minimum distance from the bar to the surface of the concrete. I argue that a cover tolerance of 3/8 in. (10 mm) means the bar is required to be no more than 3/8 in. (10 mm) closer or further from the surface than the specified cover. Is that correct?