Effects of Sand Characteristics and Fly Ash Contents on Properties of Flowable Fill

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Sand Characteristics and Fly Ash Contents on Properties of Flowable Fill

Author(s): Zhifu Yang, Karol J. Kowalski, Jan Olek, and Tommy Nantung

Publication: Materials Journal

Volume: 111

Issue: 5

Appears on pages(s): 543-552

Keywords: bleeding; controlled low-strength material; flowability; flowable fill; fly ash; penetration resistance; sand characteristics; subsidence; unconfined compressive strength

DOI: 10.14359/51686600

Date: 9/1/2014

Abstract:
This research examines the effects of sand characteristics and fly ash contents on fresh properties and on the unconfined compressive strength of flowable fill mixtures. Additionally, this research investigates the flowability of wet and dry sands and the influence of fly ash addition on this property using a number of sand sources and various levels of fly ash addition. It was found that adding fly ash into dry or wet sand substantially influenced its flowability. In addition, it was found that the flowability of sand-fly ash mixtures was influenced by such sand properties as fineness modulus and uncompacted air void content. Similarly, other flowable fill properties, such as bleeding, subsidence, penetration resistance, and unconfined compressive strength, were observed to vary with the sand property and the amount of fly ash added into the mixture.