Mechanical Resistance of Cracked Mass Concrete Repaired by Grouting: Experimental Study

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanical Resistance of Cracked Mass Concrete Repaired by Grouting: Experimental Study

Author(s): Simon Gallagher and Pierre Léger

Publication: Structural Journal

Volume: 111

Issue: 4

Appears on pages(s): 799-808

Keywords: crack repair; dam; grout injection; large-aggregate concrete; mass concrete; modulus of rupture; shear resistance; tensile resistance

DOI: 10.14359/51686581

Date: 7/1/2014

Abstract:
To evaluate the modulus of rupture and the shear strength of mass concrete repaired by grout injection, six 400 x 400 x 1250 mm (16 x 16 x 49.2 in.) concrete specimens with a maximum aggregate size of 100 mm (4 in.) were tested following ASTM C78, third-point bending test, and a loading configuration promoting large shear stresses along a vertical failure plane. ASTM C78 was performed on all virgin specimens and on repaired specimens (two repaired once and two repaired multiple times) using two different microfine injection grout mixtures with water-cement ratios (w/c) of 1.0 and 0.5. The shear test was done on two single-repaired and two multiple-repaired specimens with both grout mixtures. An average indirect tensile strength of 2.8 MPa (406 psi) was obtained for virgin specimens. This value was reduced to 1 and 0.5 MPa (145 and 72.5 psi) for specimens repaired using grout with a w/c equal to 0.5 and 1.0, respectively, regardless of the number of repairs. The shear strength of the specimens is affected by both the w/c of the injection grouts and the repaired crack width.