Cyclic Behavior of Post-Tensioned Slab-Rectangular Column Connections

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cyclic Behavior of Post-Tensioned Slab-Rectangular Column Connections

Author(s): Aris Himawan and Susanto Teng

Publication: Structural Journal

Volume: 111

Issue: 1

Appears on pages(s): 177-188

Keywords: bidirectional loading; cyclic loading; flat plate; post-tensioning; prestressed concrete slabs; punching shear; rectangular columns; slabcolumn connections.

DOI: 10.14359/51686516

Date: 1/1/2014

Abstract:
This paper describes testing of three interior post-tensioned slab-column connections having rectangular columns with a column aspect ratio of 5. The first specimen was tested under gravity load only. The second specimen was subjected to gravity and unidirectional cyclic lateral loading, and the third specimen was subjected to gravity and bidirectional cyclic lateral loading. It was confirmed that the strength and stiffness of the connections are much higher along the strong column direction than those along the weak column direction. The test results also indicate that bidirectional cyclic lateral loading significantly reduces the strength, drift capacity, ductility, and stiffness of the connections. The increase in shear strength due to prestressing for connections having rectangular columns tends to be lower compared with those having circularsquare columns. Furthermore, a modification to the ACI shear strength equation is proposed to make the prediction conservative for connections having rectangular columns.