Title: Multi-Aggregate Approach for Modeling Interfacial Transition Zone in Concrete

Author(s): Hongyan Ma and Zongjin Li

Publication: Materials Journal

Volume: 111

Issue: 2

Appears on pages(s): 189-200

Keywords: interfacial transition zone (ITZ); ITZ thickness; multi-aggregate approach; porosity; simulation; status-oriented computer model

DOI: 10.14359/51686501

Date: 3/1/2014

Abstract:
Interfacial transition zone (ITZ) has long been of particular interest in concrete technology. The limited sensitivity of experi-mental techniques makes it attractive to study ITZ using computer simulations. In this paper, a multi-aggregate approach is proposed to simulate the formation of ITZ in concrete. In light of a modified status-oriented computer model for simulating cement hydration, the evolution of ITZ is also simulated in this approach. Through simulations, the influences of several factors related to concrete mixture proportion on ITZ are investigated. It is found that ITZ thickness, as defined by the overall average porosity, can be reduced by using finer aggregate, increasing aggregate volume fraction, reducing water-cement ratio (w/c), or making the binder system finer. Following hydration, the ITZ thickness decreases continuously, but the difference of porosity between ITZ and bulk paste keeps almost constant at mature ages.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer