Early-Age Repair Material Properties

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Early-Age Repair Material Properties

Author(s): Fred R. Goodwin

Publication: Web Session

Volume: Goodwin.pdf

Issue:

Appears on pages(s):

Keywords: early-age repair properties

DOI:

Date: 4/15/2013

Abstract:
The success and durability of many concrete repair projects depend on the early-age bond, strength development, modulus development, and dimensional stability of repair binders. Common repair methods that use these materials include concrete patching, overlays, and sprayed concrete. This session will focus on the early-age properties of new and innovative repair binders as determined by laboratory evaluation, field tests, and experience. New test methods for early-age properties of repair material will also be discussed.