Prediction of Strength, Permeability, and Hydraulic Diffusivity of Ordinary Portland Cement Paste

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prediction of Strength, Permeability, and Hydraulic Diffusivity of Ordinary Portland Cement Paste

Author(s): B. Kondraivendhan and B. Bhattacharjee

Publication: Materials Journal

Volume: 111

Issue: 2

Appears on pages(s): 171-178

Keywords: compressive strength; hydraulic diffusivity; ordinary portland cement paste; permeability

DOI: 10.14359/51686452

Date: 3/1/2014

Abstract:
In this investigation, the compressive strength, permeability, and hydraulic diffusivity of ordinary portland cement (OPC) paste have been predicted from the knowledge of mixture factors, such as water-cement ratio (w/c) and curing ages. The relationships for pore size distribution (PSD) parameters, such as mean distribution radius r0.5, dispersion coefficient d, and permeable porosity P, are functions of the w/c and curing ages, and are readily available in the literature. By using these relationships, the compressive strength, permeability, and hydraulic diffusivity can be estimated from the w/c and curing age information. It is observed that the predicted compressive strength closely matches the reported experimental compressive strength. It is also observed that the estimated permeability data also closely matches the reported experimental permeability data. The predicted hydraulic diffusivity follows a similar trend, as reported in the literature.