Flexural Behavior and Strength of Reinforced Concrete Beams with Multiple Transverse Openings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Behavior and Strength of Reinforced Concrete Beams with Multiple Transverse Openings

Author(s): Bengi Aykac, Sabahattin Aykac, Ilker Kalkan, Berk Dundar, and Husnu Can

Publication: Structural Journal

Volume: 111

Issue: 2

Appears on pages(s): 267-278

Keywords: diagonal reinforcement; plastic mechanism; reinforced concrete beam; shear failure; shear reinforcement; Vierendeel truss; web crushing failure; web opening

DOI: 10.14359/51686442

Date: 3/1/2014

Abstract:
Reported are the results of experiments on 10 rectangular reinforced concrete (RC) beams with and without multiple web openings. The effects of opening geometry, the use of longitudinal stirrups in the posts between the openings, the use of diagonal reinforcement around openings, and the longitudinal reinforcement ratio on the flexural behavior of RC beams with openings were investigated. The stirrups in the posts were shown to have a significant contribution to the ductility of an RC beam with openings if no diagonal reinforcement is used. For the same reinforcement details, RC beams with circular openings were found to have higher load capacities and ductilities than beams with rectangular openings. The experiments indicated that the posts between the openings need to be prevented from undergoing shear failure to avoid Vierendeel truss action and allow a beam to develop its ductility and bending capacity.