Restoration of Historic Concrete and Masonry Structure at Lee County Courthouse

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Restoration of Historic Concrete and Masonry Structure at Lee County Courthouse

Author(s): Gabriel Carrera

Publication: Web Session

Volume: Carrera.PNG

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/15/2013

Abstract:
The main objective of this session is to present a broad perspective on the important issues related to historical structures.