Title: Concretes Made Using Portland-Limestone Cement: Comments on Performance and the Impact on Sustainability

Author(s): W. Jason Weiss

Publication: Web Session

Volume: Weiss3.pdf

Issue:

Appears on pages(s):

Keywords: portland limestone cements, sustainability

DOI:

Date: 4/15/2013

Abstract:
The construction products of tomorrow will require not only durability but also sustainability. Buildings and infrastructure will be measured by cost, quality, and environmental impact. Portland-limestone cements are products that can help the concrete industry achieve its goal of concrete being the product of choice. This session will cover the past, present, and future of limestone cements.