Three-Dimensional Optical Profilometry Analysis of the International Concrete Repair Institute Concrete Surface Profiles (CSPs)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Three-Dimensional Optical Profilometry Analysis of the International Concrete Repair Institute Concrete Surface Profiles (CSPs)

Author(s): Lauren R. Millman and James W. Giancaspro

Publication: Materials Journal

Volume: 110

Issue: 5

Appears on pages(s): 519-528

Keywords: adhesion; bond; finish; rehabilitation; repair; restoration; sand blasting; substrate; texture

DOI: 10.14359/51685903

Date: 9/1/2013

Abstract:
In this study, three-dimensional (3-D) optical profilometry was used to measure the surface amplitude height parameters of the International Concrete Repair Institute’s (ICRI’s) nine standard concrete surface profiles (CSPs). A primary objective was to evaluate the suitability of approximating the 3-D surface (areal) parameters with those extracted from two-dimensional (2-D [linear]) profiles. Four linear profile directions were considered: two diagonals as well as parallel and transverse to the longitudinal direction of the molds. The results show that, in general, the 3-D surface parameters increase through the progression of the CSP range. Estimating the 3-D surface roughness of any CSP mold using a 2-D linear profile resulted in both underestimation and overestimation errors exceeding 50%, which demonstrates the inadequacy of 2-D linear profiles to approximate the roughness of a 3-D concrete surface. The errors were reduced considerably when using a weighted average of four linear profiles to approximate the corresponding 3-D surface parameter.