Title: Ten Discussions from the September-October 2013 ACI Structural Journal

Author(s): Rivera, Luna, Whittaker; Marti-Vargas; Sanchez Filho, Lima Velasco, Silva Filho, Vaca Diez-Busch; Wang, Lu; Palieraki, Vintzileou, Silva; Wang, Lu; Mattock; He, Yi; Windisch

Publication: Structural Journal

Volume: 110

Issue: 5

Appears on pages(s): 877-897

Keywords:

DOI: 10.14359/51685840

Date: 9/1/2013

Abstract:
Disc. 109-S57/From the Sept.-Oct. 2012 ACI Structural Journal, p. 655. Development Length of Unconfined Conventional and High-Strength Steel Reinforcing Bars. (Paper by Amr Hosny, Hatem M. Seliem, Sami H. Rizkalla, and Paul Zia). Discussion by Jonathan Rivera, Bismarck Luna, and Andrew Whittaker. Disc. 109-S65/From the Nov.-Dec. 2012 ACI Structural Journal, p. 755. Bond Performance in Self-Consolidating Concrete Pretensioned Bridge Girders. (Paper by Young Hoon Kim, David Trejo, and Mary Beth D. Hueste). Discussion by José R. Martí-Vargas. Disc. 109-S66/From the Nov.-Dec. 2012 ACI Structural Journal, p. 767. Determining Slipping Stress of Prestressing Strands in Confined Sections. (Paper by Mohamed K. ElBatanouny and Paul H. Ziehl). Discussion by José R. Martí-Vargas. Disc. 109-S70/From the Nov.-Dec. 2012 ACI Structural Journal, p. 805. Shear Strength of Reinforced Concrete Girders with Carbon Fiber-Reinforced Polymer: Experimental Results. (Paper by C. Higgins, G. T. Williams, M. M. Michell, M. R. Dawson, and D. Howell). Discussion by Emil de Souza Sánchez Filho, Marta de Souza Lima Velasco, Júlio. J. Holtz Silva Filho, and Dario Vaca Diez-Busch. Disc. 109-S71/From the Nov.-Dec. 2012 ACI Structural Journal, p. 815. Longitudinal Joint Details with Tight Bend Diameter U-Bars. (Paper by Zhongguo John Ma, Qi Cao, Cheryl E. Chapman, Edwin G. Burdette, and Catherine E. W. French). Discussion by Dun Wang and Xilin Lu. Disc. 109-S73/From the Nov.-Dec. 2012 ACI Structural Journal, p. 835. Toward an Improved Understanding of Shear-Friction Behavior. (Paper by Kent A. Harries, Gabriel Zeno, and Bahram Shahrooz). Discussion by Vasiliki Palieraki, Elizabeth Vintzileou, and John F. Silva. Disc. 109-S73/From the Nov.-Dec. 2012 ACI Structural Journal, p. 835. Toward an Improved Understanding of Shear-Friction Behavior. (Paper by Kent A. Harries, Gabriel Zeno, and Bahram Shahrooz) Discussion by Dun Wang and Xilin Lu. Disc. 109-S73/From the Nov.-Dec. 2012 ACI Structural Journal, p. 835. Toward an Improved Understanding of Shear-Friction Behavior. (Paper by Kent A. Harries, Gabriel Zeno, and Bahram Shahrooz). Discussion by Alan H. Mattock. Disc. 109-S74/From the Nov.-Dec. 2012 ACI Structural Journal, p. 845. Slab Effects on Response of Reinforced Concrete Substructures after Loss of Corner Column. (Paper by Kai Qian and Bing Li). Discussion by Qingfeng He and Weijian Yi. Disc. 109-S78/From the Nov.-Dec. 2012 ACI Structural Journal, p. 889. Experimental Investigation on Punching Strength and Deformation Capacity of Shear-Reinforced Slabs. (Paper by Stefan Lips, Miguel Fernández Ruiz, and Aurelio Muttoni). Discussion by Andor Windisch.