Composite Properties of High-Strength, High-Ductility Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Composite Properties of High-Strength, High-Ductility Concrete

Author(s): Ravi Ranade, Victor C. Li, Michael D. Stults, William F. Heard, and Todd S. Rushing

Publication: Materials Journal

Volume: 110

Issue: 4

Appears on pages(s): 413-422

Keywords: engineered cementitious composites; high-ductility concrete; high-performance cementitious composite; high-strength concrete.

DOI: 10.14359/51685788

Date: 7/1/2013

Abstract:
A new fiber-reinforced cementitious composite—high-strength, high-ductility concrete (HSHDC)—has been developed at the University of Michigan, Ann Arbor, in collaboration with the U.S. Army Engineer Research and Development Center, Vicksburg, MS. The micromechanics-based design of HSHDC resulted in a unique combination of ultra-high compressive strength (166 MPa [24 ksi]), tensile ductility (3.4%), and high specific energy absorption under direct tension (greater than 300 kJ/m3 [6270 lb-ft/ft3]). The material design approach and mechanical property characterization of HSHDC under direct tension, split tension, third-point flexure, and uniaxial compression loading, along with its density and fresh properties, are reported in this paper.