Controlling Shrinkage Cracking

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Controlling Shrinkage Cracking

Author(s): by Ric Maggenti, Craig Knapp, and Sonny Fereira

Publication: Concrete International

Volume: 35

Issue: 7

Appears on pages(s): 36-41

Keywords: water, paste, aggregates, shrinkage-reducing admixtures, fibers

DOI:

Date: 7/1/2013

Abstract:
The durability of structures—especially concrete bridge decks—is compromised by the presence of cracks mainly associated with concrete shrinkage (drying shrinkage). Research and experience has demonstrated that early-age shrinkage cracking in concrete bridge decks can be significantly reduced if the mixtures have 28-day shrinkage values below 0.030%. While controlling shrinkage to these levels previously required use of low slump mixtures and large, dense aggregates, it is now possible to do so using shrinkage reducing admixtures (SRAs), water reducers, and fibers.