Design and Construction of an Internally Curing Slab

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design and Construction of an Internally Curing Slab

Author(s): Erik Holck

Publication: Web Session

Volume: Holck.pdf

Issue:

Appears on pages(s):

Keywords: Internally cured concrete, mixture proportioning, internal curing, hydration

DOI:

Date: 10/23/2012

Abstract:
In recent years, significant advancements have been made to use internal curing not only to mitigate autogenous shrinkage but also to enhance the in-place concrete performance. The objectives of this session are to assess the economics, performance, and sustainability of internal curing in various concrete applications. The following topics will be covered: mixture proportioning, internal curing methods, hydration impacts, volume change effects, mechanical properties, durability aspects, life-cycle cost analysis, impact on sustainability, and case studies that document the use of internal curing.