Meeting Extreme Demands

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Meeting Extreme Demands

Author(s): Michael H. Weber

Publication: Concrete International

Volume: 35

Issue: 5

Appears on pages(s): 52-54

Keywords: acid, temperature, durability, corrosion, strength

DOI:

Date: 5/1/2013

Abstract:
Concrete surfaces in industrial facilities may be exposed to a wide range of extreme environments, including strong acids or high temperatures. Ceratech’s activated fly ash cement concrete systems, KEMROK™ and FIREROK™, show remarkable durability in such environments.