Assessing Aggregates for Radiation-Shielding Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Assessing Aggregates for Radiation-Shielding Concrete

Author(s): Sang Y. Lee, Ann M. Daugherty, Donald J. Broton

Publication: Concrete International

Volume: 35

Issue: 5

Appears on pages(s): 31-38

Keywords: deleterious, sampling, XRF, XRD, quality

DOI:

Date: 5/1/2013

Abstract:
Petrographic examination provides an effective means to detect potentially deleterious and undesirable materials in aggregates for concrete. In this article, the authors discuss aggregates used in radiation-shielding concrete (RSC). They also cite the standards and describe the procedures for evaluating these aggregates.