Title: Effect of Horizontal Reinforcing Steel on the Strength of Molded Cylinders

Author(s): Richard D. Gaynor

Publication: Journal Proceedings

Volume: 62

Issue: 7

Appears on pages(s): 837-840

Keywords:

DOI: 10.14359/51685622

Date: 7/1/1965

Abstract:
When cores are drilled from structural concrete members, they often contain pieces of reinforcing steel. When such cores are tested for strength some laboratories attempt to remove the steel and others do not. Standard test methods are silent on this point and no data could be found in the literature.