Study of Bond Deterioration in Reinforced Concrete Beam-Column Joints

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study of Bond Deterioration in Reinforced Concrete Beam-Column Joints

Author(s): Zhu, S., and Jirsa, J. O.

Publication: Commentary Reference

Volume: 21

Issue: 33

Appears on pages(s):

Keywords:

DOI:

Date: 6/1/2011

Abstract:
PMFSEL Report No. 83-1, Department of Civil Engineering, University of Texas at Austin, TX, July 1983.