Non-Linear Material, Geometric, and Time Dependent Analysis of Reinforced and Prestressed Concrete Shells

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Non-Linear Material, Geometric, and Time Dependent Analysis of Reinforced and Prestressed Concrete Shells

Author(s): Scordelis, A. C.

Publication: Commentary Reference

Volume: 19

Issue: 10

Appears on pages(s): pp. 57-90.

Keywords:

DOI:

Date: 6/1/2011

Abstract:
Bulletin, International Association for Shells and Spatial Structures, Madrid, Spain, No. 102, Apr. 1990