Title: Shear Capacity of Reinforced Concrete Beams Using High Strength Concrete

Author(s): Elzanaty, A. H.; Nilson, A. H.; and Slate, F. O.

Publication: Commentary Reference

Volume: 11

Issue: 8

Appears on pages(s): pp. 290-296.

Keywords:

DOI:

Date: 6/1/2011

Abstract:
ACI JOURNAL, Proceedings V. 83, No. 2, Mar.-Apr. 1986