Title: Four Discussions from the May-June 2012 ACI Structural Journal and One Discussion from ACI SP-284

Author(s): Mahdi Arezoumandi, Jeffery S. Volz, Andor Windisch, Adrian E. Long, G. I. B. Rankin, Emil de Souza Sanchez Filho, Eduardo Rizzatti, Gihad Mohamad, Cary Cassiano Cavalcanti Filho, and Jacky Q. Zhang

Publication: Structural Journal

Volume: 110

Issue: 2

Appears on pages(s): 332-340

Keywords:

DOI: 10.14359/51684413

Date: 3/1/2013

Abstract:
Disc. 109-S25/From the May-June 2012 ACI Structural Journal, p. 307. Shear Behavior of Self-Consolidating Concrete Beams. (Paper by Chien-Hung Lin and Jiunn-Hung Chen). Discussion by Mahdi Arezoumandi and Jeffery S. Volz. Disc. 109-S26/From the May-June 2012 ACI Structural Journal, p. 317. Behavior of Circular and Square Reinforced Concrete Bridge Columns under Combined Loading Including Torsion. (Paper by S. Suriya Prakash, Qian Li, and Abdeldjelil Belarbi). Discussion by Andor Windisch. Disc. 109-S27/From the May-June 2012 ACI Structural Journal, p. 329. Experimental Investigations on Moment Redistribution and Punching Shear of Flat Plates. (Paper by Jung-Wook Choi and Jang-Ho Jay Kim). Discussion by Adrian E. Long and G. I. B. Rankin. Disc. 109-S31/From the May-June 2012 ACI Structural Journal, p. 369. Compressive Strength of Concrete Masonry Beams. (Paper by Thomas Ring, Sreekanta Das, and David Stubbs). Discussion by Emil de Souza Sánchez Filho, Eduardo Rizzatti, Gihad Mohamad, and Cary Cassiano Cavalcanti Filho. Disc. SP-284-21/From ACI SP-284, March 2012, p. 21-1. Serviceability and Safety of Multi-Story Flat Plate Buildings: Effect of Lateral Forces. (Paper by Amin Ghali and Ramez B. Gayed). Discussion by Jacky Q. Zhang.