Behavior of Reinforced Concrete Wide Concealed-Beam/Narrow-Column Joints under Lateral Earthquake Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Reinforced Concrete Wide Concealed-Beam/Narrow-Column Joints under Lateral Earthquake Loading

Author(s): Amer M. Elsouri and Mohamed H. Harajli

Publication: Structural Journal

Volume: 110

Issue: 2

Appears on pages(s): 205-216

Keywords: beam-column joints; bond; concealed wide beam; cyclic response; earthquake-resistant structures; seismic design; shear strength

DOI: 10.14359/51684401

Date: 3/1/2013

Abstract:
This study discusses an experimental program carried out for evaluating the behavior of reinforced concrete (RC) wide concealed-beam/narrow-column joints when subjected to lateral earthquake loading. The first part of the study focuses on as-built joints, designed and constructed without taking earthquake loads into account. The second part of the study concentrates on the seismic performance of the same joints tested in the first part, except that the reinforcement details are improved in part in accordance with ACI 318-08 provisions for earthquake-resistant structures. Four full-scale interior and exterior beam-column subassemblages were tested under quasi-static cyclic lateral loads. The joints satisfied some of the ACI 318-08 design and steel detailing requirements but still violated the dimension limitations specified in the same code or recommended by ACI 352R-02. All joint specimens developed considerably improved seismic performance, manifested by preventing or delaying joint shear failure, higher lateral load capacities, lower stiffness degradation, larger energy dissipation capacities, and a stable overall hysteretic response when compared with the as-built joints.


ALSO AVAILABLE IN:

Electronic Structural Journal