Compacted-Sand Concrete for Pavement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compacted-Sand Concrete for Pavement

Author(s): Riadh Ben Othmen, Saloua El Euch Khay, Amara Loulizi, and Jamel Neji

Publication: Concrete International

Volume: 35

Issue: 1

Appears on pages(s): 34-40

Keywords:

DOI:

Date: 1/1/2013

Abstract:
Tests show suitability of sea-dredged material as aggregate