Effects of Limestone Quarry Dust Content on Rheology and Strength of Self-Compacting Mortar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Limestone Quarry Dust Content on Rheology and Strength of Self-Compacting Mortar

Author(s): B. Benabed, S. Kenai, L. Azzouz, E. Kadri, and A. S. E. Belaidi

Publication: Symposium Paper

Volume: 289

Issue:

Appears on pages(s): 1-12

Keywords: crushed limestone dust, sand, SCM, rheology, strength

DOI: 10.14359/51684277

Date: 9/14/2012

Abstract:
Limestone quarry dusts are fine materials obtained during the process of crushing rock to produce gravel. The effects of dust content in crushed limestone sand on the properties of fresh and hardened self-compacting mortar are not well known. An experimental study was undertaken to find out the effect limestone dust content on the properties of fresh and hardened self-compacting mortar (SCM). SCM mixtures were prepared using crushed limestone sand partially replaced with limestone dust at varying percentages (0, 5, 10, 15, 20, 25 and 30%). Tests used to characterize the properties of mortars include: slump flow, flow time, viscosity measurements, compressive strength and flexural strength at 3 and 28 days of age. Results indicate that the crushed limestone dust significantly improves the rheological and mechanical properties of SCM with a content ranging from 10 to 15% of limestone dust.