Fundamental Interactions between Multi-Walled Carbon Nanotubes (MWCNT), Ca2+ and Polycarboxylate Superplasticizers in Cementitious Systems

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fundamental Interactions between Multi-Walled Carbon Nanotubes (MWCNT), Ca2+ and Polycarboxylate Superplasticizers in Cementitious Systems

Author(s): Ilina Kondofersky-Mintova and Johann Plank

Publication: Symposium Paper

Volume: 288

Issue:

Appears on pages(s): 1-12

Keywords: Carbon nanotubes, concrete, strength, polycarboxylate

DOI: 10.14359/51684245

Date: 9/14/2012

Abstract:
The fundamental interactions between polycarboxylate superplasticizers (PCEs), multi-walled carbon nanotubes (MWCNTs), Ca2+ ions and cement were investigated. Two commercial samples of MWCNTs were characterized by SEM and TEM imaging. It was found that only one sample contained mostly individual, non-agglomerated CNTs which were used in further tests. The MWCNT sample reduced cement paste flowability, but increased 28 day compressive strength by ~ 20% and tensile strength by 26%. The rela¬tively modest increase can be attributed to agglomeration of individual CNTs into large bundles (Ø ~ 900 nm, 3.51 × 10–5 in.). Agglomeration is caused by adsorption of Ca2+ ions onto the initially negatively charged surfaces of CNTs. This way, Ca2+ ions present in every cement pore solution impede maximal dispersion of CNTs in the cementitious matrix, thus limiting their potential application as nano reinforcement for concrete.