Study on the Interaction of Na-montmorillonite Clay with Polycarboxylates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on the Interaction of Na-montmorillonite Clay with Polycarboxylates

Author(s): Serina Ng and Johann Plank

Publication: Symposium Paper

Volume: 288

Issue:

Appears on pages(s): 1-15

Keywords: cement; clay; interaction; montmorillonite; polycarboxylate.

DOI: 10.14359/51684244

Date: 9/14/2012

Abstract:
The negative impact of sodium montmorillonite clay on dispersion effective¬ness of two polycarboxylates consisting of methacrylate acid: MPEG methacrylate ester at molar ratios of 6:1 and 1.5:1 was investigated. When 1% by weight of cement (bwoc) of clay was present, cement spreads decreased by up to 60% while PCE sorption soared to ~ 400 mg/g clay (~ 100 times higher than on Portland cement). The PCEs mainly undergo chemisorption by intercalation between the alumosilicate layers via their poly(ethylene oxide) side chains. Additionally, to a minor extent (~ 15%), adsorption via electrostatic attraction to the positively charged clay surfaces takes place. Polyglycols can be effectively used as a sacrificial agent to protect PCEs possessing high grafting density from the nega¬tive effects of clay, while more anionic PCEs benefit, however to a certain extent only, from the addition of highly anionic polyelectrolytes such as poly(methacrylic acid).