High Temperature Mechanical Properties of High-Strength Fly Ash Concrete with and without Fibers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High Temperature Mechanical Properties of High-Strength Fly Ash Concrete with and without Fibers

Author(s): Wasim Khaliq and Venkatesh Kodur

Publication: Materials Journal

Volume: 109

Issue: 6

Appears on pages(s): 665-674

Keywords: elastic modulus; fire resistance; fly ash concrete; high temperature properties; mechanical properties; polypropylene fibers.

DOI: 10.14359/51684164

Date: 11/1/2012

Abstract:
There is an increasing interest in the use of high-strength fly ash concrete (HFAC) due to growing environmental awareness. Knowledge of high temperature material properties is critical for evaluating the fire response of structures. This paper presents the effect of temperature on mechanical properties of plain HFAC and polypropylene fiber-reinforced HFAC (HFAC-P) with a compressive strength of approximately 70 MPa (10.1 ksi). A series of strength tests were carried out to evaluate compressive strength, tensile strength, stress-strain response, and elastic modulus of HFAC and HFAC-P in a 20 to 800°C (68 to 1472°F) temperature range. Results from mechanical property tests indicate that both HFAC and HFAC-P experience significant degradation in compressive and tensile strength, and elastic modulus with temperature. Data generated from tests are used to develop simplified relations for expressing strength and elastic modulus of HFAC and HFAC-P as a function of temperature. The proposed relations can be used as input data in computer models for evaluating fire response of structures made of HFAC with and without fibers.