SP-290: The Economics, Performance and Sustainability of Internally Cured Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: SP-290: The Economics, Performance and Sustainability of Internally Cured Concrete

Author(s): Editors: Anton K. Schindler, Jiri G. Grygar and W. Jason Weiss / Sponsored by: ACI Committee 231 and ACI Committee 213 and ACI Committee 130

Publication: Symposium Paper

Volume: 290

Issue:

Appears on pages(s): 196

Keywords:

DOI: 10.14359/51684134

Date: 10/1/2012

Abstract:
This CD consists of 14 papers presented at the ACI Fall Convention, Toronto, Canada, October 2012, and sponsored by ACI Committees 130, Sustainability of Concrete; 213, Lightweight Aggregate and Concrete; and 231, Concrete Properties at Early Ages.These papers cover the following general topics: impact on sustainability, mixture proportioning, internal curing methods and their implementation, hydration impacts, volume change effects, mechanical properties, cracking tendency, durability aspects, life-cycle cost analysis, and case studies that document the use of internal curing in full-scale production applications. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-290