50th PCI Design Awards

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 50th PCI Design Awards

Author(s):

Publication: Concrete International

Volume: 34

Issue: 10

Appears on pages(s): 30-34

Keywords:

DOI:

Date: 10/1/2012

Abstract:
In 1963, the Precast/Prestressed Concrete Institute (PCI) honored one winner and granted eight awards of merit in their first Design Awards competition. The competition has expanded greatly over the last 50 years, and this year, three juries selected 16 building projects and six bridge projects as winners.