Title: 362.1R-12: Guide for the Design and Construction of Durable Concrete Parking Structures

Author(s): ACI Committee 362

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 24

Keywords: concrete durability; construction; corrosion; curing; finishes; freezing-and-thawing resistance; nonprestressed reinforcement; parking structures; post-tensioning; precast concrete; prestressed concrete.

DOI:

Date: 9/1/2012

Abstract:
This guide presents design and construction criteria used to improve the durability of concrete parking structures. Emphasis is placed on key design criteria unique to parking structures, including structural systems, materials, structural design, durability, and construction. Also covered are cast-in-place nonprestressed concrete, cast-in-place post-tensioned concrete, and precast/prestressed concrete structural systems for use in parking structures.