Concrete Q&A: Density of Lightweight Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q&A: Density of Lightweight Concrete

Author(s):

Publication: Concrete International

Volume: 34

Issue: 8

Appears on pages(s): 74-76

Keywords:

DOI:

Date: 8/1/2012

Abstract:
Q. We have been awarded a contract to place concrete for elevated slabs on metal deck. The contract documents specify a unit weight (density) of 110 ± 3 lb/ft3 (1760 ± 50 kg/m3) for the concrete. The documents also require a hard-troweled finish. Our concrete producer has informed us that they can’t meet the specified unit weight unless air entrainment is used. To minimize the potential for blisters and delamination, we don’t want to use air entrainment. What can we do?