Title: International Workshop on Formwork Pressures Generated by Self- Consolidating Concrete

Author(s):

Publication: Concrete International

Volume: 34

Issue: 8

Appears on pages(s): 38-40

Keywords:

DOI:

Date: 8/1/2012

Abstract:
Researchers from North America and Europe recently gathered at the facilities of CBI Betonginstitutet, the Swedish Cement and Concrete Research Institute, in Stockholm, Sweden, to participate in a round-robin test program on formwork pressures generated by self-consolidating concrete (SCC).