CIH: Concrete Inspection Handbook

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: CIH: Concrete Inspection Handbook

Author(s): Published by Portland Cement Association

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 1/1/2005

Abstract:
This handbook explains the inspection provisions of the 2005 edition of ACI 318, Building Code Requirements for Structural Concrete. It explains the purpose of code requirements related to concrete construction, and gives additional background information on why these provisions are necessary. With a better understanding of code provisions comes a higher level of code enforcement, thus assuring a higher level of code compliance.