548.4M-11: Specification for Latex-Modified Concrete Overlays (Metric)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 548.4M-11: Specification for Latex-Modified Concrete Overlays (Metric)

Author(s): ACI Committee 548

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 8

Keywords: bridge decks; latex-modified concrete; mixing; resurfacing.

DOI:

Date: 6/1/2012

Abstract:
This Reference Specification covers styrene-butadiene latex-modi¬fied concrete (LMC) as an overlay on concrete bridge decks and other structures. It applies to both new construction and rehabilita¬tion of existing structures. It includes certification requirements of the latex products, storage, handling, surface preparation, mixing, application, and limitations.

Note: 548.4M-11 is only available in PDF format.