Effect of Beam Size, Casting Method, and Support Conditions on Flexural Behavior of Ultra-High-Performance Fiber-Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Beam Size, Casting Method, and Support Conditions on Flexural Behavior of Ultra-High-Performance Fiber-Reinforced Concrete

Author(s): Kay Wille and Gustavo J. Parra-Montesinos

Publication: Materials Journal

Volume: 109

Issue: 3

Appears on pages(s): 379-388

Keywords: bending strength; fiber orientation; flexural strength; residual strength; self-consolidating; steel fibers; ultra-high-performance concrete (UHPC); ultra-high-performance fiber-reinforced concrete (UHP-FRC).

DOI: 10.14359/51683829

Date: 5/1/2012

Abstract:
The flexural behavior of fiber-reinforced concretes (FRCs) is typically evaluated through standard tests of beams under either three-or four-point loading. Although these test methods are standardized, test results could vary significantly depending on specimen size, concrete casting method, and support devices used. Results from a comprehensive experimental program aimed at evaluating the influence of these test parameters on material flexural behavior are presented. The investigation focused on ultra-high-strength (>150 MPa [22 ksi]) FRC, typically referred to as ultra-high-performance FRC (UHP-FRC). By varying specimen size, casting method, and support conditions to account for those normally used by researchers in accordance with ASTM C1609/C1609M and RILEM TC 162-TDF, equivalent bending strengths as low as 10 MPa (1.4 ksi) and as high as 29 MPa (4.2 ksi) were obtained using the same UHP-FRC mixture design. The degree of restraint developed at the supports intended to work as rollers was also evaluated through finite element analyses. The use of a shear friction coefficient of 0.4, which was found to be representative of that in the “high-friction” supports used in this study, led to an increase in bending strength of approximately 30% compared to beams with no axial restraint. The test results also indicate that a more specific recommendation on the casting method is needed when using highly workable FRC, given the variability in results between beams constructed following various casting methods.