Preventive Maintenance and Sustainability of Concrete Infrastructure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Preventive Maintenance and Sustainability of Concrete Infrastructure

Author(s): Odd E. Gjorv and Vemund N. Arskog

Publication: Concrete International

Volume: 34

Issue: 5

Appears on pages(s): 36-40

Keywords:

DOI:

Date: 5/1/2012

Abstract:
Full assessment of the environmental effects of construction must include multiple impact categories