Title: Thermo-Chemo- Mechanical Cracking Assessment for Early-Age Mass Concrete Structures

Author(s): Eduardo M.R. Fairbairn, Marcos M. Silvoso, Eddy A.B. Koenders, Fernando L.B. Ribeiro, and Romildo D. Toledo Filho

Publication: Concrete International

Volume: 34

Issue: 5

Appears on pages(s): 30-35

Keywords:

DOI:

Date: 5/1/2012

Abstract:
A case study demonstrates that parallel processing allows modeling of massive and complex structures