Title: Mechanical Properties and Durability of Ultra-High-Performance Concrete

Author(s): Cornelia Magureanu, Ioan Sosa, Camelia Negrutiu, and Bogdan Heghes

Publication: Materials Journal

Volume: 109

Issue: 2

Appears on pages(s): 177-184

Keywords: compressive strength; dynamic modulus of elasticity; freezing and thawing; static modulus of elasticity; steel fibers; tensile strength; ultra-high-performance concrete.

DOI: 10.14359/51683704

Date: 3/12/2012

Abstract:
Ultra-high-performance-concrete (UHPC) is defined as concrete with compressive strength exceeding 150 N/mm2 (21,756 psi). UHPC can be fiber reinforced and displays increased mechanical performance and improved durability compared to high-strength concrete. This study presents the influence of curing/exposure conditions and concrete age on several mechanical and durability characteristics of UHPC, such as compressive strength and the static and dynamic modulus of elasticity, and the splitting and flexural tensile strengths. UHPC freezing-and-thawing resistance is also investigated. The results show that the specimens attained a compressive strength of approximately 150 N/mm2 (21,756 psi) and a modulus of elasticity greater than 50,000 N/mm2 (7,251,887 psi). The flexural characteristics depended on the fiber addition and the specimen’s dimensions. Overall, the flexural tensile strength displayed values between 14 and 34 N/mm2 (2030 to 4931 psi).